Compatibility of fracture mechanics parameters and fatigue crack growth parameters in welded joint behaviour evaluation
(Strojarski Facultet, 2013)
Problem of fracture toughness, K-Ic, determination on a crack tip localized in a welded joint is set in principle, since fracture mechanics presumes homogeneous material, not only in a crack tip surrounding but on a distance ...
Scenario razvoja loma u rotorskom bageru / Scenario of fracture development in bucket wheel excavator
(Institut za ispitivanje materijala, Beograd, 2013)
Produženi rad rotorskog bagera (BWE) u teškim radnim uslovima može dovesti do otkaza mašina. Kod veoma važnih elemenata konstrukcije, može dovesti do katastrofalnog loma. Lociranje važnih elemenata konstrukcije je od ...
An overview of application of micromechanical models in ductile fracture analysis of welded joints
(Srpsko društvo za mehaniku, Beograd, 2020)
Fracture of welded joints has been an important research and industrial topic for a long time, having in mind the key role of welded joints in ensuring the safe operation and integrity of welded structures. This work ...
Numerical and Experimental Investigations of Fracture Behaviour of Welded Joints with Multiple Defects
(MDPI, Basel, 2021)
Current standards related to welded joint defects (EN ISO 5817) only consider individual cases (i.e., single defect in a welded joint). The question remains about the behaviour of a welded joint in the simultaneous presence ...
Welded joints as critical regions in pressure vessels - case study of vinyl-chloride monomer storage tank
(Savez hemijskih inženjera, Beograd, 2018)
Welded joints are analysed as critical regions in a pressure vessel in respect to structural failure due to the elastic-plastic fracture/crack growth. To assess structural integrity of pressure vessels used in chemical ...
Impact of temperature and exploitation time on plane strain fracture toughness, k-ic, in a welded joint
(Institut za ispitivanje materijala, Beograd, 2017)
This paper presents the analysis of the impact of temperature and exploitation time on the tendency toward brittle fracture of welded joint constituents of new and exploited low-alloyed Cr-Mo steel A-387 Gr. B, by using ...
Crack initiation and propagation resistance of hsla steel welded joint constituents
(Institut za ispitivanje materijala, Beograd, 2020)
The welded joint is heterogeneous in its microstructure, mechanical and geometrical properties, thus the stress field is affected by different factors as well as by residual stress. Therefore, special procedures are needed ...
Procena integriteta i veka zavarenog panela primenom lokalnih napona / Assessment of the integrity and life of welded panel using local stresses
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2022)
Relevantne lokalne karakteristike zamornog opterećenja su najveći amplitudni napon i odgovrajauća srednja vrednost napona, koje treba odrediti za celu komponentu. Relevantna svojtva materijala se onda upoređuju sa dobijenim ...
Integrity and life assessment of welded joints made of micro-alloyed high strength steels
(Trans Tech Publications Ltd., 2020)
Structural integrity and life of welded joints made of a micro-alloyed low-carbon fine-grained normalised high strength pressure vessel steel, P460NL1 is presented [1]. The research performed within the scope of this topic ...
The Effect of Material Heterogeneity and Temperature on Impact Toughness and Fracture Resistance of SA-387 Gr. 91 Welded Joints
(MDPI, Basel, 2022)
This paper presents the analysis of the behavior of welded joints made of 9-12% Cr-Mo steel SA-387 Gr. 91. The successful application of this steel depends not only on the base metal's (BM) properties but even more on ...