Pretraživanje
Prikaz rezultata 1-10 od 22
The influence of buffer layer on the properties of surface welded joint of high-carbon steel
(Institute of Metals and Technology, 2011)
Surface welding with buffer layer is often in use because of its well-known properties of plasticity, or ability to slow crack growth initiated. However, in modern surface welding technologies, buffer layer is rarely used. ...
Curenje posude za skladištenje CO2 od austenitnog čelika / Leakage of an austenitic steel CO2 storage tank
(Institut za ispitivanje materijala, Beograd, 2012)
Posle pojave vodenih kapi na spoljašnjem zidu otvora za reviziju posude za skladištenje ugljen dioksida, detaljnom inspekcijom je otkrivena mreža prslina na prirubnici revizionog otvora, blizu zavarenog spoja između ...
Measurement of local tensile properties of welded joint using digital image correlation method
(Chemicke Listy, 2012)
M. Milosevic(a), N. Mitrovic(b), R. Jovicic(a), A. Sedmak(b), T. Maneski(b), A. Petrovic(b), and T. Aburuga(b) ((a)Innovation Center of Faculty of Mechanical Engineering, b Faculty of Mechanical Engineering, University of ...
Numerical analysis of thermal stresses in welded joint made of steels x20 and x22
(Univerzitet u Beogradu - Institut za nuklearne nauke Vinča, Beograd, 2014)
Stress calculation of steam pipeline is presented, focused on the welded joint. Numerical calculation was peiformed using the finite element method to obtain stress distribution in the welded joint made while replacing the ...
Compatibility of fracture mechanics parameters and fatigue crack growth parameters in welded joint behaviour evaluation
(Strojarski Facultet, 2013)
Problem of fracture toughness, K-Ic, determination on a crack tip localized in a welded joint is set in principle, since fracture mechanics presumes homogeneous material, not only in a crack tip surrounding but on a distance ...
Strategija održavanja zasnovana na riziku - primenljivost na cevovod / Applicability of risk-based maintenance strategy to a penstock
(Institut za ispitivanje materijala, Beograd, 2012)
Rizik od krtog loma cevovoda reverzibilne turbine je ocenjen u ranoj fazi projektovanja. Da bi se smanjili troškovi izgradnje cevovoda prihvaćen je jedan tunel. Zbog toga je za najopterećeniji segment cevovoda izabran HSLA ...
Effect of temperature and exploitation time on tensile properties and plain strain fracture toughness, K-Ic, in a welded joint
(Elsevier Science Bv, Amsterdam, 2018)
Effect of temperature and exploitation time on resistance to brittle fracture of welded joint constituents of new and 40 years exploited low-alloyed Cr-Mo steel A-387 Gr. B has been analysed. The plane strain fracture ...
Scenario razvoja loma u rotorskom bageru / Scenario of fracture development in bucket wheel excavator
(Institut za ispitivanje materijala, Beograd, 2013)
Produženi rad rotorskog bagera (BWE) u teškim radnim uslovima može dovesti do otkaza mašina. Kod veoma važnih elemenata konstrukcije, može dovesti do katastrofalnog loma. Lociranje važnih elemenata konstrukcije je od ...
Integrity and Life Assessment Procedure for a Reactor
(Elsevier Science Bv, Amsterdam, 2019)
Integrity and life assessment of structural elements or structures subjected to variable loads is necessary in order to define the control interval and removal of damages that occurred during exploitation. Integrity and ...
Risk based analysis of temperature and time effects on brittle fracture of A-387 Gr. B welded joint
(Elsevier Science Bv, Amsterdam, 2019)
Risk based analysis of temperature and time effects on fracture toughness values is applied to different regions of a welded joint made of low-alloyed Cr-Mo steel A-387 Gr. B, designed for high temperature applications. ...