Stiffener as a special design solution for pressure vessel repair

Vučetić, Trivun; Petrovski, Blagoj; Marković, Zlatan; Jeremić, Lazar; Sedmak, Aleksandar; Milošević, Nenad; Milovanović, Nikola

(Beograd : DIVK, 2022)

TY  - JOUR
AU  - Vučetić, Trivun
AU  - Petrovski, Blagoj
AU  - Marković, Zlatan
AU  - Jeremić, Lazar
AU  - Sedmak, Aleksandar
AU  - Milošević, Nenad
AU  - Milovanović, Nikola
PY  - 2022
UR  - https://machinery.mas.bg.ac.rs/handle/123456789/4279
AB  - Prikazana je popravka posude 970, jer je rizik bio veoma visok, blizu najgoreg slučaja verovatnoće i posledica. Kako položaj greške nije bio pogodan za iskopavanje i reparaturno zavarivanje, odlučeno je da se napravi ukrutni prsten,kako bi se smanjio napon u zavarenom spoju, tako da se i faktor intenziteta napona i neto napon značajno smanjuju.
AB  - The reparation of vessel 970 is shown, since the risk is
very high (close to the worst case of both probability and
consequence, being the highest). Since the defect location
was not suitable for digging out and repair welding, it was
decided to make a circumferential stiffener, to reduce the
stress acting on the welded joint, so that both the stress
intensity factor and net stress are reduced significantly.
PB  - Beograd : DIVK
T2  - Integritet i vek konstrukcija
T1  - Stiffener as a special design solution for pressure vessel repair
EP  - 266
IS  - 3
SP  - 263
VL  - 22
UR  - https://hdl.handle.net/21.15107/rcub_machinery_4279
ER  - 
@article{
author = "Vučetić, Trivun and Petrovski, Blagoj and Marković, Zlatan and Jeremić, Lazar and Sedmak, Aleksandar and Milošević, Nenad and Milovanović, Nikola",
year = "2022",
abstract = "Prikazana je popravka posude 970, jer je rizik bio veoma visok, blizu najgoreg slučaja verovatnoće i posledica. Kako položaj greške nije bio pogodan za iskopavanje i reparaturno zavarivanje, odlučeno je da se napravi ukrutni prsten,kako bi se smanjio napon u zavarenom spoju, tako da se i faktor intenziteta napona i neto napon značajno smanjuju., The reparation of vessel 970 is shown, since the risk is
very high (close to the worst case of both probability and
consequence, being the highest). Since the defect location
was not suitable for digging out and repair welding, it was
decided to make a circumferential stiffener, to reduce the
stress acting on the welded joint, so that both the stress
intensity factor and net stress are reduced significantly.",
publisher = "Beograd : DIVK",
journal = "Integritet i vek konstrukcija",
title = "Stiffener as a special design solution for pressure vessel repair",
pages = "266-263",
number = "3",
volume = "22",
url = "https://hdl.handle.net/21.15107/rcub_machinery_4279"
}
Vučetić, T., Petrovski, B., Marković, Z., Jeremić, L., Sedmak, A., Milošević, N.,& Milovanović, N.. (2022). Stiffener as a special design solution for pressure vessel repair. in Integritet i vek konstrukcija
Beograd : DIVK., 22(3), 263-266.
https://hdl.handle.net/21.15107/rcub_machinery_4279
Vučetić T, Petrovski B, Marković Z, Jeremić L, Sedmak A, Milošević N, Milovanović N. Stiffener as a special design solution for pressure vessel repair. in Integritet i vek konstrukcija. 2022;22(3):263-266.
https://hdl.handle.net/21.15107/rcub_machinery_4279 .
Vučetić, Trivun, Petrovski, Blagoj, Marković, Zlatan, Jeremić, Lazar, Sedmak, Aleksandar, Milošević, Nenad, Milovanović, Nikola, "Stiffener as a special design solution for pressure vessel repair" in Integritet i vek konstrukcija, 22, no. 3 (2022):263-266,
https://hdl.handle.net/21.15107/rcub_machinery_4279 .