Temperature and moisture distributions inside the layer of moist material placed on hot isothermal surface
(Inzhenerno-Fizicheskii Zhurnal, 2001)
The problem of contact drying of a layer of moist material placed on a hot isothermal surface is considered. A system of heat and mass transfer equations and equations for the initial and boundary conditions are proposed. ...
Analysis of the unstable fracture behaviour of a high strength low alloy steel weldment
(Pergamon-Elsevier Science Ltd, Oxford, 2004)
Local brittle zones (LBZ) cause the unstable fracture behaviour of weld metals. This threatens the safe service of welded structures and makes structural assessment procedures difficult. Therefore, the unstable fracture ...
Micromechanical coupled study of crack growth initiation criterion in pressure vessel steel
(Strength of Materials, 2004)
We present results of the combined design-theoretical investigation of the mechanism of crack growth at the onset of ductile fracture of NPP reactor pressure vessels. Micromechanical approach to the prediction of ductile ...
Determination of ductile crack initiation by magnetic emission and potential drop techniques using pre-cracked Charpy specimens
(European Structural Integrity Society, 2002)
Magnetic emission (ME) and potential drop (PD) techniques were used for instrumented Charpy impact testing in order to determine critical crack initiation properties of standard pre-cracked three-point bending specimens ...
Formation of fouling layers on a heat exchanger element exposed to warm, humid and solid loaded air streams
(Elsevier Science Inc, New York, 2002)
In consideration of the very high energy consumption of drying processes it is astonishing and disadvantageous that the majority of industrial dryers are offered and operated without energy recovery. The avoidance of fouling ...
Case study of supporting tubes failure
(Kluwer Academic Publishers, 2006)
Fracture toughness of alloyed austempered ductile iron (ADI)
(Kluwer Academic Publishers, 2006)
Plane strain fracture toughness of MP35N in aged and unaged conditions measured using modified CT specimens
(Elsevier Science Sa, Lausanne, 2003)
The multiphase alloy MP35N (35% Ni, 35% Co, 10% Mo, 20% Cr) is a high strength, high toughness alloy of choice for several safety-critical applications in aerospace, oil drilling, and biomedical industries. Several previous ...
Finite element modeling of pressure vessel with two internal surface crack
(11th International Conference on Fracture 2005, ICF11, 2005)
This paper deals with the finite element modeling of the pressure vessel with two artificial internal surface cracks, one positioned in the vessel center and the other one close to the vessel cover. Cracks are made by ...
Micromechanical coupled study of crack growth initiation criterion in Pressure vessel steel
(Problemy Prochnosti, 2004)
We present results of the combined design-theoretical investigation of the mechanism of crack growth at the onset of ductile fracture of NPP reactor pressure vessels. Micromechanical approach to the prediction of ductile ...