Determination of Residual Fatigue Life of Welded Structures at Bucket-Wheel Excavators through the Use of Fracture Mechanics
(Elsevier Science Bv, Amsterdam, 2018)
This paper presents a methodological approach for the assessment of service life of vital welded structures of a bucket-wheel excavator Sch Rs 650/5x24 ('Thyssen Krupp', Germany) boom, subjected to cyclic loading with a ...
Impact of temperature and exploitation time on plane strain fracture toughness, k-ic, in a welded joint
(Institut za ispitivanje materijala, Beograd, 2017)
This paper presents the analysis of the impact of temperature and exploitation time on the tendency toward brittle fracture of welded joint constituents of new and exploited low-alloyed Cr-Mo steel A-387 Gr. B, by using ...
Structural integrity analysis of a cracked pressure vessel
(Institut za ispitivanje materijala, Beograd, 2021)
Stress distribution, as obtained by finite element method (FEM), and corresponding fracture mechanics parameters, have been used for the integrity assessment of a pressure vessel. Once the stress distribution is known, the ...
Repair of cracks detected in cast components of vertical kaplan turbine rotor hub
(Institut za ispitivanje materijala, Beograd, 2019)
During the revitalization of the hydroelectric generating station A4 at the hydro power plant 'Djerdap 1', all of its parts are subjected to non-destructive testing. Cracks are detected in cast part of generator rotor hub, ...
Analiza rasta prsline u zonama spoja frikciono zavarenog mešanjem korišćenjem proširene metode konačnih elemenata / Crack growth analysis in friction stir welded joint zones using extended finite element method
(Institut za ispitivanje materijala, Beograd, 2013)
U ovom radu je prikazana analiza rasta prsine u zonama zavarenog spoja izvedenog postupkom frikcionog zavarivanja mešanjem (FSW). Ploče od legure aluminijuma 2024-T351 su sučeono zavarene primenom postupka FSW. Ploče su ...
Curenje posude za skladištenje CO2 od austenitnog čelika / Leakage of an austenitic steel CO2 storage tank
(Institut za ispitivanje materijala, Beograd, 2012)
Posle pojave vodenih kapi na spoljašnjem zidu otvora za reviziju posude za skladištenje ugljen dioksida, detaljnom inspekcijom je otkrivena mreža prslina na prirubnici revizionog otvora, blizu zavarenog spoja između ...
Ocena integriteta rezervoara sa mikroprslinama u zavarenom spoju / Integrity assessment of tanks with microcracks in welded joints
(Institut za ispitivanje materijala, Beograd, 2013)
Tokom eksploatacije rezervoara za skladištenje tečnog ugljendioksida ukazala se potreba za ugradnjom dva nova priključka u jedno od danaca. Rezervoar je izrađen od mikrolegiranog čelika, a priključci od visokolegiranog ...
Metodološki pristup proceni integriteta i veka rotacione opreme u hidroelektrani - turbinsko vratilo / Methodological approach to integrity assessment and service life of rotating equipment at hydropower plant: Turbine shaft
(Institut za ispitivanje materijala, Beograd, 2013)
Horizontalne Kaplanove turbine su instalirane u hidroelektrani 'ĐERDAP 2', 10 jedinica ukupne snage 28 MW. Uzimajući u obzir činjenicu da se zamor pojavio u mnogim komponentama, sprovedeno je istraživanje uticaja režima ...