Damages of burner pipes due to the working conditions and its repair welding
2018
Preuzimanje 🢃
Autori
Tanasković, DrakčeĐorđević, Branislav R.
Gajin, Marko
Aranđelović, Mihajlo
Gostović, Nemanja
Konferencijski prilog (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
Repair welding represents the activity that restores the working capability of machine or construction caused by some damage due to working or environmental condition. Damages of burner pipes, part of the facility "Cold Rolling Mill" Steelwork in Smederevo, which appeared on welded joints during the manufacturing of the burner, and its repairing are presented in this paper. The damages occurred on welded joints along the weld as a result of the working conditions that burner was exposed to. Due to high temperatures that can reach up to 850 degrees C and "explosion" during gas burning, a crack may appear on the inner side of the burner. The base material of the burner pipes is stainless steel X12NiCrSi35-16. Repair welding is preceded by a series of operations, and one of them is the selection of an electrode. It turned out that inadequate selection of the electrode for repair welding had contributed to the occurrence of cracks on welded joints. Selecting a new electrode and examining i...ts characteristics, as well as performing test welding of pipe that is still in exploitation, had confirmed the importance of proper selection of materials for repairing of burner pipes.
Ključne reči:
steel X12NiCrSi35-16 / repair welding / damages / burner pipeIzvor:
Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity, 2018, 13, 404-409Izdavač:
- Elsevier Science Bv, Amsterdam
Finansiranje / projekti:
- Integritet opreme pod pritiskom pri istovremenom delovanju zamarajućeg opterećenja i temperature (RS-MESTD-Technological Development (TD or TR)-35011)
DOI: 10.1016/j.prostr.2018.12.067
ISSN: 2452-3216
WoS: 000459860900066
Scopus: 2-s2.0-85064690998
Institucija/grupa
Inovacioni centarTY - CONF AU - Tanasković, Drakče AU - Đorđević, Branislav R. AU - Gajin, Marko AU - Aranđelović, Mihajlo AU - Gostović, Nemanja PY - 2018 UR - https://machinery.mas.bg.ac.rs/handle/123456789/2837 AB - Repair welding represents the activity that restores the working capability of machine or construction caused by some damage due to working or environmental condition. Damages of burner pipes, part of the facility "Cold Rolling Mill" Steelwork in Smederevo, which appeared on welded joints during the manufacturing of the burner, and its repairing are presented in this paper. The damages occurred on welded joints along the weld as a result of the working conditions that burner was exposed to. Due to high temperatures that can reach up to 850 degrees C and "explosion" during gas burning, a crack may appear on the inner side of the burner. The base material of the burner pipes is stainless steel X12NiCrSi35-16. Repair welding is preceded by a series of operations, and one of them is the selection of an electrode. It turned out that inadequate selection of the electrode for repair welding had contributed to the occurrence of cracks on welded joints. Selecting a new electrode and examining its characteristics, as well as performing test welding of pipe that is still in exploitation, had confirmed the importance of proper selection of materials for repairing of burner pipes. PB - Elsevier Science Bv, Amsterdam C3 - Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity T1 - Damages of burner pipes due to the working conditions and its repair welding EP - 409 SP - 404 VL - 13 DO - 10.1016/j.prostr.2018.12.067 ER -
@conference{ author = "Tanasković, Drakče and Đorđević, Branislav R. and Gajin, Marko and Aranđelović, Mihajlo and Gostović, Nemanja", year = "2018", abstract = "Repair welding represents the activity that restores the working capability of machine or construction caused by some damage due to working or environmental condition. Damages of burner pipes, part of the facility "Cold Rolling Mill" Steelwork in Smederevo, which appeared on welded joints during the manufacturing of the burner, and its repairing are presented in this paper. The damages occurred on welded joints along the weld as a result of the working conditions that burner was exposed to. Due to high temperatures that can reach up to 850 degrees C and "explosion" during gas burning, a crack may appear on the inner side of the burner. The base material of the burner pipes is stainless steel X12NiCrSi35-16. Repair welding is preceded by a series of operations, and one of them is the selection of an electrode. It turned out that inadequate selection of the electrode for repair welding had contributed to the occurrence of cracks on welded joints. Selecting a new electrode and examining its characteristics, as well as performing test welding of pipe that is still in exploitation, had confirmed the importance of proper selection of materials for repairing of burner pipes.", publisher = "Elsevier Science Bv, Amsterdam", journal = "Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity", title = "Damages of burner pipes due to the working conditions and its repair welding", pages = "409-404", volume = "13", doi = "10.1016/j.prostr.2018.12.067" }
Tanasković, D., Đorđević, B. R., Gajin, M., Aranđelović, M.,& Gostović, N.. (2018). Damages of burner pipes due to the working conditions and its repair welding. in Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity Elsevier Science Bv, Amsterdam., 13, 404-409. https://doi.org/10.1016/j.prostr.2018.12.067
Tanasković D, Đorđević BR, Gajin M, Aranđelović M, Gostović N. Damages of burner pipes due to the working conditions and its repair welding. in Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity. 2018;13:404-409. doi:10.1016/j.prostr.2018.12.067 .
Tanasković, Drakče, Đorđević, Branislav R., Gajin, Marko, Aranđelović, Mihajlo, Gostović, Nemanja, "Damages of burner pipes due to the working conditions and its repair welding" in Procedia Structural Integrity - ECF22 - Loading and environmental effects on structural integrity, 13 (2018):404-409, https://doi.org/10.1016/j.prostr.2018.12.067 . .